"Add bubble wrap" is the standard answer to fragile shipping, and it is incomplete in a way that costs money.
Fragile goods fail three distinct ways in transit, and bubble wrap only addresses one of them properly. The transit test standard the parcel industry uses tests those three separately, because they are separate problems with separate fixes.
The other thing worth saying up front: a lot of what circulates about fragile packaging in India is invented. The widely repeated claims that Amazon requires 5-ply corrugated board with partitions for glass, and that Meesho bans courier bags for fragile items, appear in agency guides with no citation and in no platform document. This guide is built on the things that are published — a test procedure, a dunnage rule, and a board measurement — and it says so where nothing is.
The three ways things break
Impact. The parcel is dropped. Force transmits through the packaging into the product. This is the failure everyone designs for, and the one cushioning solves — by decelerating the product over a distance rather than stopping it against a wall.
Compression. The parcel sits under a stack, in a van, a warehouse aisle or a dark store bin, with weight on it for hours. Cushioning does very little here. This is a structural problem, answered by board strength and by internal structure that gives the box something to load through.
Vibration. Hours of low-level movement over road surfaces. Products abrade against the box or each other, caps work loose, seals gradually fail. This is the quiet one: the product arrives intact but scuffed, or the lid arrives half open. Prevented by immobilisation, not by padding.
You will see confident claims about which of the three causes most e-commerce damage in India. No one publishes that number, and the people who quote it are usually selling the fix. What you can do is measure it on your own returns, by SKU and by pack.

What the published transit standard actually tests
There is a formal standard, and it is more specific than the "ISTA 3A" name-drop suggests.
ISTA Procedure 3A sits in ISTA's 3 Series, which ISTA calls a General Simulation Performance Test Procedure. Its scope, in ISTA's own words: "Test Procedure 3A covers testing of individual packaged-products weighing 70 kilograms (150 pounds) or less when prepared for shipment via a parcel delivery carrier." It splits packages into four types — standard, small, flat and elongated — because a long thin parcel and a small cube fail differently. A "small" package is under 13,000 cm³, no longer than 350 mm and no heavier than 4.5 kg; a "flat" one has a shortest dimension of 200 mm or less.
The sequence, and the ASTM method ISTA calls up for each:
| Sequence | What it simulates | Method |
|---|---|---|
| Preconditioning, then atmospheric conditioning | Warehouse humidity and temperature, because damp board is weaker board | ASTM D4332 |
| Drop — nine drops, height varying with packaged-product weight | Handling and sortation impacts | ASTM D5276 |
| Random vibration, with and without a top load | Road transport, loaded and stacked | ASTM D4728 |
| Random vibration under low pressure (optional) | Air freight | ASTM D6653 |
| Drop — a further eight drops, including a hazard impact | Later-stage handling on an already-fatigued pack | ASTM D5276 |
| Rotational edge drop, 200 mm | A heavy parcel tipped onto one edge | ASTM D6179 |
| Full rotational flat drop | A parcel toppling flat | — |
| Concentrated impact, hazard box dropped 400 mm (flat packages) | Something sharp landing on a flat parcel | ASTM D5265 |
| Bridge impact (elongated packages) | A long parcel supported at its ends and struck in the middle | ASTM D5265 |
| Leak test, 8 hours | Liquids finding their way out | — |
Two things are worth pulling out of that table.
There is no standalone compression test in 3A. The compression case is handled by running the vibration sequence with a top load on the parcel. If stacking strength is your risk, you measure that separately, on the box — more on how, below.
Drop height is not a single number. It varies with the weight of the packaged product, which is why "we drop-test from X" is a claim to be curious about.
ISTA asks for one sample as a minimum, and recommends "two (2) or more" for fragile items or products containing liquids — which tells you something about how repeatable a single result is.
The bench version, and what it is worth
Testing to 3A means a lab, a drop tester, a vibration table and a bill. For a small brand it is usually not the first spend. A crude bench version catches gross failures, and it is much better than nothing:
- Pack a real unit exactly as a customer would receive it, invoice and all.
- Drop it from about 90 cm onto a hard floor — once on each face, once on a corner, once on an edge. That height is not arbitrary: Amazon's own US FBA rules require a bubble-wrapped item to "pass a 3-foot drop test on a hard surface without the contents breaking", and three feet is 91 cm. Amazon's India manual gives no such figure.
- Put a realistic load on it. Amazon caps inbound cartons at 15 kg, so one loaded carton on top of yours is a fair stand-in for one layer of a stack.
- Shake it. If you can hear or feel the product moving, it will abrade or work loose over hours of road transport.
- Open it and inspect the product, not the box. A box that survived while the contents scuffed is still a failure.
Do this before your first large order rather than after your first complaints. Be clear about what it is, though: a screen, not a substitute for a standard. It does not condition the board, it does not vibrate the pack for hours, and one unit is one unit.
The single most common failure: the product touches the box wall
If any part of your product contacts the outer box, an impact on that face transmits straight into the product with nothing absorbing it. Cushioning that surrounds the product but leaves one contact point is decoration around a weak spot.
So the working rule for a breakable item is that it should be suspended, not packed — cushioning on all six faces, including top and bottom, and nothing touching a wall.
Which has an immediate sizing consequence: a box sized snugly to your product cannot be cushioned properly. You have to size up deliberately, then fill the gap.
How much gap? The honest answer is that the published figures are rules of thumb, not measurements:
- Amazon's US FBA guidance says: "Use 2 inches of cushioning between each of your items and the inside of the box." That is about 5 cm.
- Packaging distributors commonly advise adding 1–2 inches of clearance on all sides for bubble, foam or paper.
- The arithmetic that follows from either is: padded internal dimension = bare product dimension + (2 × padding thickness).
- Amazon's India seller manual gives no clearance figure at all.
The engineering answer is different in kind. Cushion thickness is properly derived from the product's own fragility, the weight it puts on the cushion per unit of bearing area, and the drop height you are designing against — which is what cushion curves are for. A rule of thumb is what you use when you have not done that work. Treat 2.5–5 cm as a starting point, then test the pack you actually ship.
how to size a box before you order it
What that clearance costs, in the sizes you can actually buy
This is the part most fragile-packaging advice leaves out. Sizing up to make room for cushioning is not free — you pay for it in board once, and in volumetric weight on every order, forever.
Take a product measuring 10 × 6 × 6 cm and weighing 300 g, and work it through Evenpack's stock corrugated range (board prices on evenpack.co in October 2026):
| Cushioning per face | Internal space needed | Nearest stock box | Volumetric weight | Billed at | Board, printed one side, 500 pack |
|---|---|---|---|---|---|
| Snug, about 5 mm | 11 × 7 × 7 cm | 5 × 5 × 3 in | 0.25 kg | 0.5 kg | ₹12.00 |
| 25 mm (1 in) | 15 × 11 × 11 cm | 6 × 6 × 6 in | 0.71 kg | 1.0 kg | ₹15.90 |
| 50 mm (2 in) | 20 × 16 × 16 cm | 8 × 8 × 8 in | 1.68 kg | 2.0 kg | ₹21.65 |
Volumetric weight here uses the usual domestic formula — length × width × height in centimetres divided by 5000 — with the courier billing whichever is higher, actual or volumetric, rounded up to the next 500 g slab. Check your own contract, because the divisor varies; some services use 4000 or 4500, which pushes the figure up.
Read across the bottom row: protecting that product properly costs ₹9.65 more per box and three extra 500 g freight slabs on every order. The one-inch row costs ₹3.90 and one extra slab.
That is not an argument against protecting it. It is an argument for knowing the number, because "just use a bigger box" is advice with a recurring invoice attached. If your product does not need 2 inches, do not buy 2 inches.

the same volumetric maths across three formats
Board strength: ask for edge crush, not GSM
Against compression, the thing that matters is board strength, and grammage does not measure it.
Edge crush test (ECT) measures the cross-direction crushing resistance of corrugated board, as force per unit width, in kilonewtons per metre or pounds per inch. It is determined under ISO 3037. ECT is the property that predicts how a box behaves in a stack.
Box compression test (BCT) is the direct measurement of the finished box, reported in kgf or newtons. The McKee formula estimates BCT from the board's ECT, the board thickness and the box perimeter — a useful approximation with known limits, not a substitute for testing the box.
Bursting strength (the Mullen test) is the pressure needed to rupture the board, in kPa or lb/in². It is a puncture and rupture measure. In India it is often quoted as a burst factor, which is burst strength × 1000 ÷ grammage — note the grammage in the denominator, which is exactly why a GSM figure on its own tells you very little.
Amazon's own inbound carton specification is written this way rather than in GSM: acceptable containers are described as "an RSC (regular slotted carton), B flute, ECT-32 (edge crush test), 200BH (burst strength)". A structure, a flute, an edge crush figure and a burst figure. No ply count, and no grammage.
So what about 5-ply? 5-ply adds a second fluted layer and a third liner, and double-wall board is made for higher stacking strength and puncture resistance. That is real. But ply describes a construction, not a strength — two 5-ply boards made from different papers perform differently, and a well-specified 3-ply can out-perform a poor 5-ply. If crushing is your failure mode, specify the ECT or the box compression figure you need and let the supplier tell you what construction delivers it.
Evenpack's stock corrugated range is 3-ply E-flute at 150 + 100 + 150 GSM, in brown kraft and white, and it ships flat for you to fold. That is a flute and a grammage, which is what stock is usually sold on. If you need a measured figure, ask for it before you commit — and see the checklist at the end of this post, because it is a fair question to put to any supplier including this one.

how corrugated board is built, ply by ply
What the marketplaces actually say about fragile goods
Less than you have been told, and not where you have been told it.
Amazon publishes category guidance to all Indian sellers as advice. In its own words: "Use sufficient bubble wrap for items like glass, porcelain, clocks, and mirrors, before placing them into cardboard boxes or corrugates." Each item wrapped individually, with "sufficient cushioning so the products do not move within the package". Heavier fragile goods double-boxed, with orientation and damage-warning labels. Electronics: "Mobiles, MP3 players, camera, shavers and other electronic items should be bubble-wrapped and double-boxed using corrugates of the right size." Liquids: seal the lids, and where there is no double seal, wrap the container "in a fully sealable strong plastic bag or plastic sheet, and seal all the seams".
Amazon's harder rules are for stock going into a fulfilment centre, not for parcels you pack and hand to a courier yourself. There, breakable items "must be in a solid six-sided box so that the item is not exposed in any way", and "All items must be individually wrapped to prevent damage from other items within the container". Cartons are capped at 15 kg.
No Amazon document names a ply count, a board grade or corrugated partitions for any category. The "5-ply plus bubble wrap plus partitions for glass" line that circulates as an Amazon requirement is not in Amazon's seller blog or its India shipment preparation manual.
Meesho publishes no fragile-goods rule. The claim that Meesho forbids courier bags for fragile items comes from the same uncited agency material. Meesho's published packaging instructions are about branding and MRP, not protection.
Flipkart publishes nothing usable in public on packaging. Its guidance sits inside the seller portal.
None of which means a courier bag is a sensible pack for a wine glass. It is not — a flexible bag offers essentially no crush protection, and that is a structural fact rather than a marketplace rule. Make the decision on the failure mode, and if you sell on a marketplace, read the rule in your own portal rather than in a blog.
what each marketplace actually publishes
The one dunnage rule that is published
Amazon's India shipment preparation manual is unusually specific about void fill, and the distinction it draws is the useful one:
"Use large-sized dunnage, such as air pillows, full sheets of paper, sheet foam or bubble wrap. Do not use loose fill of any kind, such as Styrofoam peanuts or shredded paper."
Its accepted list is foam and polythene rolls, air pillows and full sheets of paper. Its rejected list is styrofoam peanuts, crinkle wrap and shredded paper.
Notice where the line falls. It is not drawn between materials — bubble, air pillows, sheet foam and full sheets of paper are treated as interchangeable. It is drawn between large-sized dunnage and loose fill, because loose fill settles in transit and leaves the product free to move by the time it arrives.
Within the accepted group, the materials do differ, and the differences are functional rather than a ranking:
- Bubble film conforms to an awkward shape and cushions on every face at once. Its weakness is that a punctured or crushed cell stops working, so a thin layer that has been squeezed into a tight box may be doing less than it looks.
- Inflatable air pillows fill volume cheaply and quickly. They are void fill first and cushioning second: under a concentrated load they move aside rather than decelerate anything.
- Full sheets of paper, crumpled, hold position better than any loose material and go into paper recycling with the box. They are bulkier and heavier for the same void, so you need more of them.
- Moulded pulp is a fitted insert rather than void fill. It holds the product in one fixed position, which is primarily a vibration and orientation answer. It needs a tool, so it belongs at volume, not at a first run.
What you cannot do is compare any of these by brochure. The measurement that compares cushioning materials is a cushion curve: the peak deceleration transmitted to the product, plotted against the load the product puts on the cushion per unit of bearing area, for a stated material thickness and drop height. A supplier who has curves will show you them. "Superior protection" is not a number.
What Evenpack supplies, and what it does not
Worth being plain about, because this post tells you to buy several things and only some of them come from here.
Stock, and cushioned as supplied:
- Bubble-padded paper courier bags and bubble-padded envelopes — 6 × 6, 8 × 10, 12 × 10 and 16 × 12 inches, paper outer with a bubble-cushion lining, self-sealing, printed on one side or plain, from 100 pieces. The 6 × 6 starts at ₹17.75 per piece printed in a 100 pack and ₹6.35 in a 2,000 pack (₹13.25 and ₹4.75 plain), on evenpack.co in October 2026.
- Rigid mailers in 175 and 215 GSM, 8 × 6 to 17.5 × 13 inches from 100 pieces, and a heavier 430 GSM range, 9.5 × 5.3 to 18 × 14 inches from 500 pieces — for flat things whose failure mode is bending rather than breaking.
Stock, as the outer box:
- Corrugated shipping boxes, 3-ply E-flute, 150 + 100 + 150 GSM, 5 × 5 × 3 to 12 × 9 × 6 inches in brown (six of the sizes also in white), flat-packed, from 50 pieces.
- Mailer boxes, same board, 4 × 4 × 1.5 to 9 × 6 × 3 inches, from 50 pieces.
Not supplied by Evenpack: bubble film on the roll, air pillows, paper void fill, foam and moulded pulp. Those come from a protective-packaging supplier, and this post is not pretending otherwise.
Custom development: 5-ply and 7-ply board, non-stock sizes and internal partitions are quoted as a custom job rather than bought off the shelf, so allow the lead time — fully custom developments typically run 10 to 20 business days from proof approval.
browse stock corrugated boxes and mailer boxes
What to use, by product
The outer pack is the decision this post can help with. The protection inside it is a separate purchase, listed here so the spec is complete rather than implied.
| Product | Outer pack | Protection inside |
|---|---|---|
| Small item, already robust or in its own rigid box | Bubble-padded courier bag or envelope | The integral bubble lining |
| Cosmetics, skincare, liquids | Corrugated box | Cushioning on all faces, plus a sealed bag round the container so a leak stays contained |
| Glass, ceramics, single item | Corrugated box sized up for clearance | Cushioning on all six faces, nothing touching a wall |
| Multiple glass or ceramic items | Corrugated box | Dividers so the items cannot meet, then cushioning |
| Electronics | Corrugated box, double-boxed for heavier units | Bubble wrap, per Amazon's own category guidance |
| Flat items that must arrive flat — prints, framed pieces | Rigid mailer (175, 215 or 430 GSM) | Board rigidity plus corner protection |
| Anything where crushing in a stack is the risk | Box specified on edge crush or box compression | Internal structure that carries load, not more padding |
bubble-padded paper courier bags
Three things that quietly go wrong
Loose fill settles. This is the one failure mode a major platform has written a rule about: Amazon refuses loose fill of any kind on inbound stock and asks for large-sized dunnage instead. If a platform that handles that volume of parcels will not accept it, it is a reasonable signal for your own packing bench.
Tape fails before board does. A share of "damaged in transit" claims are boxes that opened rather than boxes that broke. Seal along every seam, and on a heavier fragile parcel treat the bottom as carefully as the top — it is the seam that carries the weight when the parcel is lifted.
Over-packing creates its own problem. Cushioning held under constant compression takes a permanent set and stops cushioning; a product wedged in tightly can also be stressed by the pack itself. The target is immobilised without pressure, which is not the same as tight.
The economics
Fragile packaging costs more per unit, and it looks like an obvious saving to trim. Run the numbers before you do.
A damaged delivery costs you the product, the outbound shipping, the replacement product, the replacement shipping, the support time, and often the review and the repeat customer. Against that, a few rupees of board and cushioning is cheap. But as the clearance table above shows, "a few rupees" understates it once volumetric weight is counted, so the decision deserves an actual sum rather than a slogan.
The discipline that settles it is measuring your own damage rate by SKU and packaging type. If it is near zero on a line, you may be over-protecting and can trim. If it is not, you are already paying for it — in replacements rather than in board. Anyone who offers you an industry damage rate instead is quoting a number no one publishes.
talk through a protection spec for your product
FAQ
What is the best packaging for fragile items?
It depends which failure mode you are facing. Impact is prevented by cushioning with enough thickness to decelerate the product, compression by board strength and internal structure, and vibration by immobilising the product so it cannot move. Most breakable items need a corrugated box sized up so there is cushioning on all six faces and nothing touching a wall.
Does Amazon require 5-ply corrugated boxes for glass?
No. No Amazon document names a ply count or a board grade for any product category. Amazon's India seller blog asks for sufficient bubble wrap for glass, porcelain, clocks and mirrors, individual wrapping and double-boxing of heavier items. The nearest thing Amazon publishes to a board specification is for inbound fulfilment-centre cartons: an RSC in B flute, ECT-32 or 200 burst.
How much clearance should there be between the product and the box?
The published rules of thumb are 1 to 2 inches on every face — Amazon's US FBA guidance says to use 2 inches of cushioning between each item and the inside of the box. Padded internal dimension equals the bare product dimension plus twice the padding thickness. Treat that as a starting point, not a specification: cushion thickness is properly derived from the product's fragility and the drop height you are designing against.
Can I ship fragile items in a courier bag?
For anything breakable, no. A flexible bag offers essentially no crush protection. There is no published Indian marketplace rule banning it — the widely quoted Meesho rule has no source — but the structural argument stands on its own, and Amazon's published rule for breakables going into its fulfilment centres is a solid six-sided box.
How do I test whether my packaging protects the product?
The formal route is ISTA Procedure 3A, for individual packaged products of 70 kg or less shipped through a parcel delivery carrier, which runs conditioning, two drop sequences, random vibration with and without a top load, rotational drops, an impact test and an 8-hour leak test for liquids. Informally: pack a real unit, drop it from about 90 cm onto each face plus a corner and an edge, put a loaded carton on top of it, shake it for movement, then open it and inspect the product rather than the box.
Why do my products arrive scuffed even though the box is undamaged?
That is vibration damage. Over hours of transit a product that can move inside its box abrades against the walls or against other items. The fix is immobilisation rather than more padding — the product should not be able to shift at all, which is why void fill that settles is unreliable for fragile goods.
Name the failure mode first
Work out which failure mode you are actually facing. Cushioning stops impact, board strength stops crushing, immobilisation stops vibration, and they are not interchangeable.
Then size the box up deliberately so there is room to protect the product, price what that sizing does to your freight before you standardise on it, and drop-test a real unit before you commit to a thousand. And when someone quotes you a requirement, ask where it is published.